Steel grade designation | Name | THICKNESS from _ to in mm |
WIDTH from _ to in mm |
---|---|---|---|
DT4 | Soft magnetic iron | 0.6-1.6 | 800-1250 |
Steel grade | C [%] | Si [%] | Mn [%] | P [%] | S [%] | Cr [%] | Ni [%] | Cu [%] | Mo[%] | Ti[%] |
---|---|---|---|---|---|---|---|---|---|---|
DT4 | ≤0.025 | ≤0.2 | ≤0.3 | ≤0.02 | ≤0.02 | ≤0.1 | ≤0.2 | ≤0.2 | - | - |
Steel grade designation | Name | THICKNESS from _ to in mm |
WIDTH from _ to in mm |
---|---|---|---|
DT4A | Soft magnetic iron | 0.6-1.6 | 800-1250 |
Steel grade | C [%] | Si [%] | Mn [%] | P [%] | S [%] | Cr [%] | Ni [%] | Cu [%] | Mo[%] | Ti[%] |
---|---|---|---|---|---|---|---|---|---|---|
DT4A | ≤0.01 | ≤0.1 | ≤0.25 | ≤0.015 | ≤0.01 | ≤0.1 | ≤0.05 | ≤0.05 | - | ≤0.02 |
Steel grade designation | Name | THICKNESS from _ to in mm |
WIDTH from _ to in mm |
---|---|---|---|
DT4C | Soft magnetic iron | 0.6-1.6 | 800-1250 |
Steel grade | C [%] | Si [%] | Mn [%] | P [%] | S [%] | Cr [%] | Ni [%] | Cu [%] | Mo[%] | Ti[%] |
---|---|---|---|---|---|---|---|---|---|---|
DT4C | ≤0.025 | ≤0.2 | ≤0.3 | ≤0.02 | ≤0.02 | ≤0.1 | ≤0.2 | ≤0.2 | - | - |
Steel grade designation | Name | THICKNESS from _ to in mm |
WIDTH from _ to in mm |
---|---|---|---|
DT4E | Soft magnetic iron | 0.6-1.6 | 800-1250 |
Steel grade | C [%] | Si [%] | Mn [%] | P [%] | S [%] | Cr [%] | Ni [%] | Cu [%] | Mo[%] | Ti[%] |
---|---|---|---|---|---|---|---|---|---|---|
DT4E | ≤0.025 | ≤0.2 | ≤0.3 | ≤0.02 | ≤0.02 | ≤0.1 | ≤0.2 | ≤0.2 | - | - |